Material Specifications

TEST TYPE EPDM SILICONE
Advance Ozone Resistance

Test at 500 pphm

70 hours 70 hours
High Temperature

Intermittent: 275+ degrees F 500+ degrees F
  Continuous: 212+ degrees F 437+ degrees F
Low Temperature

Resistance Tested to: 65- degrees F 100- degrees F
Tensile Strength: 1,450 psi 700 psi