Material Specifications
Flasher
Masterflash
Retrofit
Dektite
Retrofit
Masterflash
Round Base Flashing/Flasher® Materials Chart
Test Type
EPDM
Silicone
Advance Ozone Resistance Test at 500 pphm
70 hours
70 hours
High Temperature
Intermittent:
275+ degrees F
500+ degrees F
Continuous:
212+ degrees F
437+ degrees
F
Low Temperature
Resistance Tested to:
65- degrees F
100- degrees F
Tensile Strength:
1,450 psi
700 psi
Square Base Flashing/Masterflash® Materials Chart
Test Type
EPDM
Silicone
Advance Ozone Resistance Test at 500 pphm
70 hours
70 hours
High Temperature
Intermittent:
275+ degrees F
500+ degrees F
Continuous:
212+ degrees F
437+ degrees F
Low Temperature
Resistance Tested to:
65- degrees F
100- degrees F
Tensile Strength:
1,450 psi
700 psi
Round Base Retrofit/Retrofit Dektite® Materials Chart
Test Type
EPDM
Silicone
Advance Ozone Resistance Test at 500 pphm
70 hours
70 hours
High Temperature
Intermittent:
275+ degrees F
500+ degrees F
Continuous:
212+ degrees F
437+ degrees F
Low Temperature
Resistance Tested to:
65- degrees F
100- degrees F
Tensile Strength:
1,450 psi
700 psi
Square Base Retrofit (Retrofit Masterflash®) Materials Chart
Test Type
EPDM
Silicone
Advance Ozone Resistance Test at 500 pphm
70 hours
70 hours
High Temperature
Intermittent:
275+ degrees F
500+ degrees F
Continuous:
212+ degrees F
437+ degrees F
Low Temperature
Resistance Tested to:
65- degrees F
100- degrees F
Tensile Strength:
1,450 psi
700 psi
Search:
Can't Find It?
Contact Us
We Will Find it
For You!
800-334-9815
Join Our Email List
Mailing List:
About Us
Terms
Privacy Policy
Contact Us
Site Map
Copyright 2010 Protech Products, Inc.